Solution
1)Melt PBAT compounding with PLA or PPC
The melt PBAT material with temperature 240℃ is fed into twin screw extruder by a melt pump, and add the PLA or PPC pellets and chain extender additive into extruder by the loss-in-weight feeder. This is direct compounding which can save 40% energy and better dispersion, comparing with PBAT pellet compounding with PLA or PPC
2)PLA/PBS compounding with starch powder
Model | L/D | Screw Speed (rpm) | Motor Power (KW) | Specific Torque( T/A3) | Capacity Range ( kg/hr) |
CJWH-65 | 40~56 | 300 | 75 | 9 | 240 |
CJWH-75 | 40~56 | 300 | 132 | 9 | 440 |
CJWH-95 | 40~56 | 300 | 250 | 9 | 820 |
CJWS-75 | 40~56 | 300 | 160 | 11 | 550 |
CJWS-95 | 40~56 | 300 | 315 | 11 | 1060 |